UNE-EN ISO 2566-1:2022
Current
The latest, up-to-date edition.
Steel - Conversion of elongation values - Part 1: Carbon and low-alloy steels (ISO 2566-1:2021, Corrected version 2022-06)
Hardcopy , PDF
Spanish, Castilian, English
20-07-2022
This document specifies a method of converting room temperature percentage elongations after fracture obtained on various proportional and non-proportional gauge lengths to other gauge lengths.Formula (1), on which conversions are based, is considered to be reliable when applied to carbon, carbon manganese, molybdenum and chromium molybdenum steels within the tensile strength range 300 to 700 N/mm2 and in the hot-rolled, hot-rolled and normalized or annealed conditions, with or without tempering.These conversions are not applicable to:a) cold reduced steels;b) quenched and tempered steels;c) austenitic steels.These conversions are not applicable when the gauge length exceeds 25S0 or where the width to thickness ratio of the test piece exceeds 20.
| Committee |
CTN 36
|
| DocumentType |
Standard
|
| Pages |
44
|
| PublisherName |
Asociación Española de Normalización
|
| Status |
Current
|
| Standards | Relationship |
| EN ISO 2566-1:2021 | Identical |
| ISO 2566-1:2021 | Identical |
Access your standards online with a subscription
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.