AS 2552-1982
Current
The latest, up-to-date edition.
Steel sheet and strip - Terne (lead-tin alloy) coated
Hardcopy , PDF 1 User , PDF 3 Users , PDF 5 Users , PDF 9 Users
English
09-08-1982
Specifies flat steel sheet and strip, in thicknesses from 0.6 to 2mm and up to 1220mm wide, terne-coated by the hot dip process. Provision is made for four grades of steel and three classes of terne coating.
Committee |
MT-001
|
DocumentType |
Standard
|
ISBN |
0 7262 2573 8
|
Pages |
10
|
ProductNote |
Reconfirmed 27/05/2016.This standard has been reconfirmed in Australia in 2016 and remains current in New Zealand. Reconfirmation Notice 27/05/2016
|
PublisherName |
Standards Australia
|
Status |
Current
|
Supersedes |
This standard specifies requirements for flat steel sheet and strip terne (8 percent to 20 percent tin, remainder lead) coated by the hot-dip process, in thicknesses from 0.6 mm up to and including 2.0 mm and up to 1220 mm wide. It provides for four grades of steel, the chemical composition and mechanical properties of which are in accordance with the grades of cold rolled material in AS 1595. Provision is made for three classes of terne coating based on the mass per unit area of the coating metal applied.NOTE: Guidelines to purchasers on requirements that must he specified by the purchaser and those that must be agreed at the time of enquiry and/or order are given in Appendix A.The material shall be supplied in accordance with the requirements of this Section 1. The steel base shall comply with the requirements of Section 2.The terne coating shall comply with the requirements of Section 3.
First published (as AS G28) 1969.
First published as AS 2552 1982
AS 1391-2007 | Metallic materials - Tensile testing at ambient temperature (Reconfirmed 2017) |
AS 1815.1-2007 | Metallic materials - Rockwell hardness test Test method (scales A, B, C, D, E, F, G, H, K, N, T) (Reconfirmed 2017) |
AS 2338-2004 | Preferred dimensions of wrought metal products |
AS/NZS 1365:1996 | Tolerances for flat-rolled steel products (Reconfirmed 2016) |
AS 1397-2001 | Steel sheet and strip - Hot-dipped zinc-coated or aluminium/zinc-coated |
AS 2025.1-1977 | Method for Rockwell superficial hardness test - Testing of metals, N and T scales |
AS 2505.1-2004 | Metallic materials Sheet, strip and plate - Bend tests |
AS 1812-1975 | Lead ingot |
AS/NZS 1595:1998 | Cold-rolled, unalloyed, steel sheet and strip (Reconfirmed 2016) |
AS 1650-1989 | Hot-dipped galvanized coatings on ferrous articles |
AS 1213-1982 | Iron and steel - Methods of sampling |
AS 4647-2005 | Domestic diaphragm gas meters |
AS 3513-1987 | Information processing systems - Data communication - High-level data link control balanced classes of procedures - Data-link layer address resolution/negotiation in switched environments |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.