ASTM B 954 : 2015 : REDLINE
Superseded
A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.
View Superseded by
Standard Test Method for Analysis of Magnesium and Magnesium Alloys by Atomic Emission Spectrometry
01-05-2023
English
03-11-2015
CONTAINED IN VOL. 02.02, 2015 Describes the analysis of magnesium and its alloys by atomic emission spectrometry.
Committee |
B 07
|
DocumentType |
Redline
|
Pages |
9
|
PublisherName |
American Society for Testing and Materials
|
Status |
Superseded
|
SupersededBy |
1.1This test method describes the analysis of magnesium and its alloys by atomic emission spectrometry. The magnesium specimen to be analyzed may be in the form of a chill cast disk, casting, sheet, plate, extrusion or some other wrought form or shape. The elements covered in the scope of this method are listed in the table below.
Element | Mass Fraction Range (Wt %) |
Aluminum | 0.001 to 12.0 |
Beryllium | 0.0001 to 0.01 |
Boron | 0.0001 to 0.01 |
Cadmium | 0.0001 to 0.05 |
Calcium | 0.0005 to 0.05 |
Cerium | 0.01 to 3.0 |
Chromium | 0.0002 to 0.005 |
Copper | 0.001 to 0.05 |
Dysprosium | 0.01 to 1.0 |
Erbium | 0.01 to 1.0 |
Gadolinium | 0.01 to 3.0 |
Iron | 0.001 to 0.06 |
Lanthanum | 0.01 to 1.5 |
Lead | 0.005 to 0.1 |
Lithium | 0.001 to 0.05 |
Manganese | 0.001 to 2.0 |
Neodymium | 0.01 to 3.0 |
Nickel | 0.0005 to 0.05 |
Phosphorus | 0.0002 to 0.01 |
Praseodymium | 0.01 to 0.5 |
Samarium | 0.01 to 1.0 |
Silicon | 0.002 to 5.0 |
Silver | 0.001 to 0.2 |
Sodium | 0.0005 to 0.01 |
Strontium | 0.01 to 4.0 |
Tin | 0.002 to 0.05 |
Titanium | 0.001 to 0.02 |
Yttrium | 0.02 to 7.0 |
Ytterbium | 0.01 to 1.0 |
Zinc | 0.001 to 10.0 |
Zirconium | 0.001 to 1.0 |
Note 1:The mass fraction ranges given in the above scope are estimates based on two manufacturers observations and data provided by a supplier of atomic emission spectrometers. The range shown for each element does not demonstrate the actual usable analytical range for that element. The usable analytical range may be extended higher or lower based on individual instrument capability, spectral characteristics of the specific element wavelength being used and the availability of appropriate reference materials.
1.2This test method is suitable primarily for the analysis of chill cast disks as described in Sampling Practice B953. Other forms may be analyzed, provided that: (1) they are sufficiently massive to prevent undue heating, (2) they allow machining to provide a clean, flat surface which creates a seal between the specimen and the spark stand, and (3) reference materials of a similar metallurgical condition (spectrochemical response) and chemical composition are available.
1.3This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Specific safety and health statements are given in Section 10.
ASTM B 91 : 2017 : REDLINE | Standard Specification for Magnesium-Alloy Forgings |
ASTM B 403 : 2012 : REDLINE | Standard Specification for Magnesium-Alloy Investment Castings |
MIL-DTL-32333 Base Document:2009 | ARMOR PLATE, MAGNESIUM ALLOY, AZ31B, APPLIQUE |
ASTM B 93/B93M : 2015 : REDLINE | Standard Specification for Magnesium Alloys in Ingot Form for Sand Castings, Permanent Mold Castings, and Die Castings |
SAE AMS 4484 : 2013 | MAGNESIUM ALLOY CASTINGS, PERMANENT MOLD, 9.0AL - 2.0ZN (AZ92A-T6), SOLUTION AND PRECIPITATION HEAT TREATED |
SAE AMS2355M | QUALITY ASSURANCE, SAMPLING AND TESTING, ALUMINUM ALLOYS AND MAGNESIUM ALLOY, WROUGHT PRODUCTS (EXCEPT FORGING STOCK), AND ROLLED, FORGED, OR FLASH WELDED RINGS |
SAE AMS 4434 : 2017 | MAGNESIUM ALLOY CASTINGS, SAND, 9.0AL - 2.0ZN (AZ92A-T6), SOLUTION AND PRECIPITATION HEAT TREATED |
ASTM B 107/B107M : 2013 : REDLINE | Standard Specification for Magnesium-Alloy Extruded Bars, Rods, Profiles, Tubes, and Wire |
SAE AMS 4424 : 2014 | Magnesium Alloy Castings, Sand 6.0Al - 3.0Zn (AZ63-T6) Solution and Precipitation Heat Treated |
SAE AMS4490K | Magnesium Alloy Castings, Die 9.0Al - 0.70Zn (AZ91D, Temper F) As Cast |
SAE AMS 4483 : 2013 | MAGNESIUM ALLOY CASTINGS, PERMANENT MOLD, 10AL (AM100A-T6), SOLUTION AND PRECIPITATION HEAT TREATED |
SAE AMS 4437 : 2014 | MAGNESIUM ALLOY CASTINGS, SAND, 8.7AL - 0.70ZN (AZ91C-T6), SOLUTION HEAT TREATED AND AGED |
SAE AMS 4418 : 2012 | MAGNESIUM ALLOY, SAND CASTINGS, 2.5AG - 2.1DI - 0.70ZR (QE22A-T6), SOLUTION AND PRECIPITATION HEAT TREATED |
SAE AMS 4439 : 2012 | MAGNESIUM ALLOY CASTINGS, 4.2ZN - 1.2 RARE EARTHS - 0.7ZR (ZE41A-T5), PRECIPITATION HEAT TREATED |
ASTM B 90/B90M : 2015 : REDLINE | Standard Specification for Magnesium-Alloy Sheet and Plate |
SAE AMS 4417 : 2018 | CASTINGS, SAND, MAGNESIUM ALLOY, 1.5AG - 2.1DI - 0.08CU - 0.70ZR (EQ21A - T6), SOLUTION AND PRECIPITATION HEAT TREATED |
SAE AMS 4371 : 2015 | MAGNESIUM ALLOY, PLATE, 4.0Y - 2.25ND - 0.5ZR (WE43C - T5), PRECIPITATION HEAT TREATED |
SAE AMS 4429 : 2012 | MAGNESIUM ALLOY CASTINGS, SAND 2.8ND - 1.4GD - 0.4ZN - 0.6ZR (EV31A - T6), SOLUTION AND PRECIPITATION HEAT TREATED |
ASTM B 92/B92M : 2017 : REDLINE | Standard Specification for Unalloyed Magnesium Ingot and Stick For Remelting |
ASTM B 953 : 2013 : REDLINE | Standard Practice for Sampling Magnesium and Magnesium Alloys for Spectrochemical Analysis |
SAE AMS 4362 : 2014 | FORGINGS, MAGNESIUM ALLOY, 5.5ZN - 0.45ZR (ZK60A-T5), PRECIPITATION HEAT TREATED |
SAE AMS4452E | MAGNESIUM ALLOY, INVESTMENT CASTINGS, 8.7AL - 0.70ZN - 0.22MN (AZ91C-T6) SOLUTION AND PRECIPITATION HEAT TREATED |
SAE AMS 4442 : 2012 | MAGNESIUM ALLOY SAND CASTINGS, 3.2 RARE EARTHS - 2.5ZN - 0.70ZR (EZ33A-T5), PRECIPITATION HEAT TREATED |
SAE AMS4453F | MAGNESIUM ALLOY, INVESTMENT CASTINGS, 9.0AL - 2.0ZN (AZ92A-T6) SOLUTION AND PRECIPITATION HEAT TREATED |
SAE AMS4455G | MAGNESIUM ALLOY, INVESTMENT CASTINGS, 10AL (AM100A-T6) SOLUTION AND PRECIPITATION HEAT TREATED |
ASTM F 3160 : 2016 | Standard Guide for Metallurgical Characterization of Absorbable Metallic Materials for Medical Implants |
ASTM B 199 : 2017 : REDLINE | Standard Specification for Magnesium-Alloy Permanent Mold Castings |
SAE AMS 4426 : 2013 | CASTINGS, SAND, MAGNESIUM ALLOY 5.1Y - 3.0RE - 0.70ZR (WE54-T6) SOLUTION AND PRECIPITATION HEAT TREATED |
SAE AMS 4427 : 2012 | MAGNESIUM ALLOY CASTINGS, SAND, 4.0Y - 2.3ND - 0.7ZR (WE43B - T6), SOLUTION AND PRECIPITATION HEAT TREATED |
SAE AMS 4485A : 2017 | MAGNESIUM ALLOY, EXTRUSIONS 4.0Y - 2.25ND - 0.5ZR (WE43C - T5) PRECIPITATION HEAT TREATED |
SAE AMS4443H | MAGNESIUM ALLOY, SAND CASTINGS, 4.5ZN - 0.75ZR (ZK51A-T5) PRECIPITATION HEAT TREATED |
ASTM F 3268 : 2018 | Standard Guide for <emph type="bdit">in vitro</emph> Degradation Testing of Absorbable Metals |
ASTM E 826 : 2014 : REDLINE | Standard Practice for Testing Homogeneity of a Metal Lot or Batch in Solid Form by Spark Atomic Emission Spectrometry |
ASTM B 953 : 2013 : REDLINE | Standard Practice for Sampling Magnesium and Magnesium Alloys for Spectrochemical Analysis |
ASTM E 305 : 2013 : REDLINE | Standard Practice for Establishing and Controlling Atomic Emission Spectrochemical Analytical Curves |
ASTM E 1257 : 2016 : REDLINE | Standard Guide for Evaluating Grinding Materials Used for Surface Preparation in Spectrochemical Analysis |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.