• DEFSTAN 03-29/2(1997) : 1997

    Superseded A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.

    PROTECTION OF METALLIC SPRINGS AGAINST CORROSION

    Available format(s): 

    Superseded date:  31-01-2002

    Language(s): 

    Published date:  12-01-2013

    Publisher:  UK Ministry of Defence Standards

    Sorry this product is not available in your region.

    Add To Cart

    Table of Contents - (Show below) - (Hide below)

    1 Scope
    2 WARNING
    3 Related documents
    4 Definition
    5 Information to be supplied to the processor
    6 Process control
    7 Factors affecting the choice of protective
             treatments
    8 General requirements in applying protective
             treatments
    9 Protective treatments for various materials
    TABLE A Tensile strengths
    TABLE B Protective treatments for use where surface
             electrical conductivity is of paramount
             importance
    TABLE C Protective treatments for protection against
             corrosion

    Abstract - (Show below) - (Hide below)

    Provides the requirements for the protection of all types of metallic springs against corrosion and is intended for use in conjunction with, but not to supersede, relevant design documents or other instructions.

    General Product Information - (Show below) - (Hide below)

    Development Note Supersedes DEFSTAN 03-29/1(1988) & DG-10 (07/2003)
    Document Type Standard
    Publisher UK Ministry of Defence Standards
    Status Superseded
    Superseded By
    Supersedes

    Standards Referenced By This Book - (Show below) - (Hide below)

    DEFSTAN 03-11/3(1995) : 1995 PHOSPHATE TREATMENT OF IRON AND STEEL
    DEFSTAN 03-4/4(1998) : 1998 THE PRE-TREATMENT AND PROTECTION OF STEEL ITEMS OF SPECIFIED MAXIMUM TENSILE STRENGTH EXCEEDING 1450 MPA

    Standards Referencing This Book - (Show below) - (Hide below)

    DEFSTAN 03-19/2(1994) : 1994 ELECTRO-DEPOSITION OF CADMIUM
    DEFSTAN 03-9/2(1992) : 1992 ELECTRO-DEPOSITION OF SILVER
    DTD 931 : AUG 70 RHODIUM PLATING
    BS EN 22063:1994 Metallic and other inorganic coatings. Thermal spraying. Zinc, aluminium and their alloys
    BS 7195(1989) : 1989 GUIDE FOR PREVENTION OF CORROSION OF METALS CAUSED BY VAPOURS FROM ORGANIC MATERIALS
    DEFSTAN 01-4/1(1972) : 1972 GUIDE TO SELECTION OF METALLIC MATERIALS FOR SPRINGS
    DEFSTAN 03-28(PT1)/2(1995) : 1995 PHYSICAL VAPOUR DEPOSITION OF METALS - PART 1: PHYSICAL VAPOUR DEPOSITION OF ALUMINIUM FOR PROTECTION AGAINST CORROSION
    DEFSTAN 03-8/2(1992) : 1992 ELECTRO-DEPOSITION OF TIN
    DEFSTAN 03-11/3(1995) : 1995 PHOSPHATE TREATMENT OF IRON AND STEEL
    DTD 940 : NOV 68 THE CADMIUM COATING OF VERY STRONG STEEL PARTS BY VACUUM EVAPORATION
    DEFSTAN 03-4/3(1991) : 1991 THE PRE-TREATMENT AND PROTECTION OF STEEL ITEMS OF SPECIFIED MAXIMUM TENSILE STRENGTH EXCEEDING 1450 MPa
    DEFSTAN 03-20/2(1994) : 1994 AMD 1 1996 ELECTRO-DEPOSITION OF ZINC
    DEFSTAN 03-28(PT2)/2(1995) : 1995 PHYSICAL VAPOUR DEPOSITION OF METALS - PART 2: PHYSICAL VAPOUR DEPOSITION OF CADMIUM FOR PROTECTION AGAINST CORROSION
    DEFSTAN 03-27/1(1987) : 1987 ELECTRODEPOSITION OF NICKEL FOR ENGINEERING PURPOSES
    BS 2W 12:1989 Specification for preformed zinc coated carbon steel wire rope (metric and inch series)
    DEFSTAN 03-17/2(1992) : 1992 ELECTRO - DEPOSITION OF GOLD
    PD 6484:1979 Commentary on corrosion at bimetallic contacts and its alleviation
    DEFSTAN 03-33/1(1993) : 1993 CHROMATE PASSIVATION OF CADMIUM AND ZINC SURFACES
    BS 427:1990 Method for Vickers hardness test and for verification of Vickers hardness testing machines
    DEFSTAN 03-2/3(1995) : 1995 CLEANING AND PREPARATION OF METAL SURFACES
    DEFSTAN 00-970/VOL1/1(1983) : AMD 14 DESIGN AND AIRWORTHINESS REQUIREMENTS FOR SERVICE AIRCRAFT - AEROPLANES
    DEFSTAN 00-970/VOL2/1(1984) : 1984 DESIGN AND AIRWORTHINESS REQUIREMENTS FOR SERVICE AIRCRAFT - ROTORCRAFT
    DEFSTAN 01-5/11(1996) : 1996 FUELS, LUBRICANTS AND ASSOCIATED PRODUCTS
    DEFSTAN 03-21/1(1983) : 1983 MECHANICAL METHODS FOR THE INDUCEMENT OF COMPRESSIVE SURFACE RESIDUAL STRESSES
    • Access your standards online with a subscription

      Features

      • Simple online access to standards, technical information and regulations
      • Critical updates of standards and customisable alerts and notifications
      • Multi - user online standards collection: secure, flexibile and cost effective