1 Scope
2 Normative references
3 Terms and Definitions
4 Designation
5 Condition of delivery
6 Tolerances on thickness
7 Tolerances on width
7.1 General
7.2 Sheet and wide strip
7.3 Slit wide strip of width less than 600 mm
8 Tolerances on length
9 Tolerances on flatness
9.1 General
9.2 Steel grades with specified minimum yield strength
Re < 260 Mpa
9.3 Steel grades with specified minimum yield strength
260 MPa <= Re < 340 Mpa
9.4 Steel grades with specified minimum yield strength
Re >= 340 MPa
10 Tolerances on out-of-squareness
11 Tolerances on edge camber
12 Superimposition of dimensions
Bibliography
Applies to cold rolled uncoated and electrolytically zinc or zinc-nickel coated low carbon and high yield strength steel flat products for cold forming with a minimum thickness of 0,35 mm and, unless otherwise agreed at the time of ordering, less than or equal to 3 mm thick, delivered in sheet, wide strip, slit wide strip or cut lengths obtained from slit wide strip or sheet.
| DocumentType |
Standard
|
| Pages |
14
|
| PublisherName |
National Standards Authority of Ireland
|
| Status |
Current
|
| Supersedes |
| Standards | Relationship |
| NBN EN 10131 : 2007 | Identical |
| NS EN 10131 : 2ED 2006 | Identical |
| NEN EN 10131 : 2006 | Identical |
| BS EN 10131:2006 | Identical |
| NF EN 10131 : 2006 | Identical |
| EN 10131:2006 | Identical |
| DIN EN 10131:2006-09 | Equivalent |
| UNE-EN 10131:2007 | Identical |