1. SCOPE
2. APPLICABLE DOCUMENTS
3. TECHNICAL REQUIREMENTS
4. QUALITY ASSURANCE PROVISIONS
5. PREPARATION FOR DELIVERY
6. ACKNOWLEDGMENT
7. REJECTIONS
8. NOTES

Specifies a corrosion and heat resistant nickel alloy in the form of sand castings.

Committee
AMS F
DocumentType
Standard
Pages
7
ProductNote
THIS STANDARD IS NOW STABILIZED
PublisherName
SAE International
Status
Current
Supersedes

SAE AMS2645K FLUORESCENT PENETRANT INSPECTION
ASTM E 446 : 2015 : REDLINE Standard Reference Radiographs for Steel Castings Up to 2 in. (50.8 mm) in Thickness
SAE AMS 2804 : 2001 IDENTIFICATION - CASTINGS
SAE AMS2635D RADIOGRAPHIC INSPECTION
SAE AMS 2694 : 2013 IN-PROCESS WELDING OF CASTINGS
ASTM E 10 : 2017-05 TEST METHOD FOR BRINELL HARDNESS OF METALLIC MATERIALS
SAE AMS 2350 : 1989 STANDARDS AND TEST METHODS
SAE AMS 2360 : 2012 ROOM TEMPERATURE TENSILE PROPERTIES OF CASTINGS
MIL-STD-794 Revision E:1982 PART AND EQUIPMENT, PROCEDURES FOR PACKAGING AND PACKING OF
ASTM E 354 : 2014 : REDLINE Standard Test Methods for Chemical Analysis of High-Temperature, Electrical, Magnetic, and Other Similar Iron, Nickel, and Cobalt Alloys
SAE AMS 2268 : 1988 CHEMICAL CHECK ANALYSIS LIMITS, CAST NICKEL AND NICKEL ALLOYS

Access your standards online with a subscription

Features

  • Simple online access to standards, technical information and regulations.

  • Critical updates of standards and customisable alerts and notifications.

  • Multi-user online standards collection: secure, flexible and cost effective.