DIN EN 13523-27:2009-10
Superseded
A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.
COIL COATED METALS - TEST METHODS - PART 27: RESISTANCE TO HUMID POULTICE (CATAPLASM TEST)
Hardcopy , PDF
07-03-2021
English
01-01-2009
National foreword
National Annex NA (informative) - Bibliography
European foreword
1 Scope
2 Normative references
3 Terms and definitions
4 Principle
5 Apparatus and materials
6 Sample preparation
7 Procedure
8 Expression of results
9 Test report
Bibliography
Defines a procedure for evaluating the resistance of an organic coating on a metallic substrate (coil coating) in conditions of extreme humidity (acid, alkaline and/or neutral).
DocumentType |
Standard
|
Pages |
10
|
PublisherName |
German Institute for Standardisation (Deutsches Institut für Normung)
|
Status |
Superseded
|
Standards | Relationship |
EN 13523-27:2017 | Identical |
EN ISO 4628-2:2016 | Paints and varnishes - Evaluation of degradation of coatings - Designation of quantity and size of defects, and of intensity of uniform changes in appearance - Part 2: Assessment of degree of blistering (ISO 4628-2:2016) |
EN 13523-0:2014 | Coil coated metals - Test methods - Part 0: General introduction |
EN 1396:2015 | Aluminium and aluminium alloys - Coil coated sheet and strip for general applications - Specifications |
EN ISO 4628-10:2016 | Paints and varnishes - Evaluation of degradation of coatings - Designation of quantity and size of defects, and of intensity of uniform changes in appearance - Part 10: Assessment of degree of filiform corrosion (ISO 4628-10:2016, Corrected version 2016-06-01) |
ISO 4628-3:2016 | Paints and varnishes — Evaluation of degradation of coatings — Designation of quantity and size of defects, and of intensity of uniform changes in appearance — Part 3: Assessment of degree of rusting |
EN ISO 4628-3:2016 | Paints and varnishes - Evaluation of degradation of coatings - Designation of quantity and size of defects, and of intensity of uniform changes in appearance - Part 3: Assessment of degree of rusting (ISO 4628-3:2016) |
EN 10169:2010+A1:2012 | Continuously organic coated (coil coated) steel flat products - Technical delivery conditions |
ISO 4628-10:2016 | Paints and varnishes — Evaluation of degradation of coatings — Designation of quantity and size of defects, and of intensity of uniform changes in appearance — Part 10: Assessment of degree of filiform corrosion |
ISO 4628-5:2016 | Paints and varnishes — Evaluation of degradation of coatings — Designation of quantity and size of defects, and of intensity of uniform changes in appearance — Part 5: Assessment of degree of flaking |
ISO 3696:1987 | Water for analytical laboratory use — Specification and test methods |
EN ISO 3696:1995 | Water for analytical laboratory use - Specification and test methods (ISO 3696:1987) |
EN ISO 4628-5:2016 | Paints and varnishes - Evaluation of degradation of coatings - Designation of quantity and size of defects, and of intensity of uniform changes in appearance - Part 5: Assessment of degree of flaking (ISO 4628-5:2016) |
DIN ISO 3696:1991-06 | WATER FOR ANALYTICAL LABORATORY USE - SPECIFICATION AND TEST METHODS |
ISO 4628-2:2016 | Paints and varnishes Evaluation of degradation of coatings Designation of quantity and size of defects, and of intensity of uniform changes in appearance Part 2: Assessment of degree of blistering |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.