I.S. EN 60317-42:1998
Current
The latest, up-to-date edition.
SPECIFICATIONS FOR PARTICULAR TYPES OF WINDING WIRES - PART 42: POLYESTER-AMIDE-IMIDE ENAMELLED ROUND COPPER WIRE, CLASS 200
Hardcopy , PDF
English
01-01-1998
For Harmonized Standards, check the EU site to confirm that the Standard is cited in the Official Journal.
Only cited Standards give presumption of conformance to New Approach Directives/Regulations.
Dates of withdrawal of national standards are available from NSAI.
FOREWORD
INTRODUCTION
1 Scope
2 Normative references
3 Definitions and general notes on methods of test
4 Dimensions
5 Electrical resistance
6 Elongation
7 Springiness
8 Flexibility and adherence
9 Heat shock
10 Cut-through
11 Resistance to abrasion (nominal conductor diameters
from 0,250 mm up to and including 2,500 mm)
12 Resistance to solvents
13 Breakdown voltage
14 Continuity of insulation
15 Temperature index
16 Resistance to refrigerants
17 Solderability
18 Heat or solvent bonding
19 Dielectric dissipation factor
20 Resistance to transformer oil
21 Loss of mass
22 High temperature failure
30 Packaging
Annex ZA (normative) Normative references to international
publications with their corresponding European
publications
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.