1 Scope
2 Normative references
3 Definitions
4 Properties
Tables
Defines the test requirements for the physical properties of the harmonised cross-linked PVC sheathing compound.
Committee |
GEL/20/17
|
DevelopmentNote |
Supersedes BS 7655-12.2(1997) and 02/202798 DC. (01/2006)
|
DocumentType |
Standard
|
Pages |
10
|
PublisherName |
British Standards Institution
|
Status |
Current
|
Supersedes |
Standards | Relationship |
NEN EN 50363-10-1 : 2006 | Identical |
DIN EN 50363-10-1 : 2006 | Identical |
SN EN 50363-10-1 : 2005 | Identical |
UNE-EN 50363-10-1:2006 | Identical |
NF EN 50363-10-1 : 2006 | Identical |
EN 50363-10-1:2005 | Identical |
I.S. EN 50363-10-1:2005 | Identical |
NBN EN 50363-10-1 : 2006 | Identical |
EN 50290-2-20:2016 | Communication cables - Part 2-20: Common design rules and construction - General |
IEC 60811-3-1:1985 | Common test methods for insulating and sheathing materials ofelectric cables - Part 3: Methods specific to PVC compounds -Section One: Pressure test at high temperature - Tests forresistance to cracking |
HD 627 S1:1996/A2:2005 | MULTICORE AND MULTIPAIR CABLES FOR INSTALLATION ABOVE AND BELOW GROUND |
IEC 60684-2:2011 | Flexible insulating sleeving - Part 2: Methods of test |
EN 50267-2-1:1998 | Common test methods for cables under fire conditions - Tests on gases evolved during combustion of materials from cables - Part 2-1: Procedures - Determination of the amount of halogen acid gas |
IEC 60811-4-1:2004 | Insulating and sheathing materials of electric and optical cables - Common test methods - Part 4-1: Methods specific to polyethylene and polypropylene compounds - Resistance to environmental stress cracking - Measurement of the melt flow index - Carbon black and/or mineral filler content measurement in polyethylene by direct combustion - Measurement of carbon black content by thermogravimetric analysis (TGA) - Assessment of carbon black dispersion in polyethylene using a microscope |
HD 22.10 S2:2007 | Cables of rated voltages up to and including 450/750 V and having cross-linked insulation - Part 10: EPR insulated and polyurethane sheathed flexible cables |
EN 60684-2:2011 | Flexible insulating sleeving - Part 2: Methods of test |
EN 60811-3-2 : 95 AMD 2 2004 | INSULATING AND SHEATHING MATERIALS OF ELECTRIC AND OPTICAL CABLES - COMMON TEST METHODS - PART 3-2: METHODS SPECIFIC TO PVC COMPOUNDS - LOSS OF MASS TEST - THERMAL STABILITY TEST |
EN 50290-2-27 : 2002 COR 2010 | COMMUNICATION CABLES - PART 2-27: COMMON DESIGN RULES AND CONSTRUCTION - HALOGEN FREE FLAME RETARDANT THERMOPLASTIC SHEATHING COMPOUNDS |
EN 60811-1-3:1995/A1:2001 | INSULATING AND SHEATHING MATERIALS OF ELECTRIC CABLES - COMMON TEST METHODS - PART 1-3: GENERAL APPLICATION - METHODS FOR DETERMINING THE DENSITY - WATER ABSORPTION TESTS - SHRINKAGE TEST |
HD 620 : 2010 | DISTRIBUTION CABLES WITH EXTRUDED INSULATION FOR RATED VOLTAGES FROM 3,6/6 (7,2) KV UP TO AND INCLUDING 20,8/36 (42) KV |
EN 50290-2-29:2016 | Communication cables - Part 2-29: Common design rules and construction - Crosslinked polyethylene insulation compounds: instrumentation, control and field bus cables |
HD 603 S1:1994/A3:2007 | DISTRIBUTION CABLES OF RATED VOLTAGE 0,6/1 KV |
EN 50290-2-23:2013 | COMMUNICATION CABLES - PART 2-23: COMMON DESIGN RULES AND CONSTRUCTION - POLYETHYLENE INSULATION FOR MULTI-PAIR CABLES USED IN ACCESS TELECOMMUNICATION NETWORKS: OUTDOOR CABLES |
EN 50290-2-26 : 2002 AMD 1 2007 | COMMUNICATION CABLES - PART 2-26: COMMON DESIGN RULES AND CONSTRUCTION - HALOGEN FREE FLAME RETARDANT INSULATION COMPOUNDS |
HD 22.15 : 200S2 | CABLES OF RATED VOLTAGES UP TO AND INCLUDING 450/750 V AND HAVING CROSS-LINKED INSULATION - PART 15: MULTICORE CABLES INSULATED AND SHEATHED WITH HEAT RESISTANT SILICONE RUBBER |
EN 60811-3-1 : 95 AMD 2 2001 | INSULATING AND SHEATHING MATERIALS OF ELECTRIC CABLES - COMMON TEST METHODS - METHODS SPECIFIC TO PVC COMPOUNDS - PRESSURE TEST AT HIGH TEMPERATURE - TESTS FOR RESISTANCE TO CRACKING |
HD 21.14 : 2003 | CABLES OF RATED VOLTAGE UP TO AND INCLUDING 450/750 V AND HAVING THERMOPLASTIC INSULATION - PART 14: FLEXIBLE CABLES (CORDS), INSULATED AND SHEATHED WITH HALOGEN-FREE THERMOPLASTIC COMPOUNDS |
HD 626 S1:1996/A2:2002 | OVERHEAD DISTRIBUTION CABLES OF RATED VOLTAGE U[O]/U(U[M]): 0,6/1 (1,2) KV |
EN 50290-2-28:2002 | Communication cables - Part 2-28: Common design rules and construction - Filling compounds for filled cables |
HD 21.15 : 200S1 | CABLES OF RATED VOLTAGES UP TO AND INCLUDING 450/750 V AND HAVING THERMOPLASTIC INSULATION - PART 15: SINGLE CORE CABLES, INSULATED WITH HALOGEN-FREE THERMOPLASTIC COMPOUND, FOR FIXED WIRING |
IEC 60811-1-2:1985 | Common test methods for insulating and sheathing materials of electric cables - Part 1: Methods for general application - Section Two: Thermal ageing methods |
EN 60811-4-1:2004 | Insulating and sheathing materials of electric and optical cables - Common test methods - Part 4-1: Methods specific to polyethylene and polypropylene compounds - Resistance to environmental stress cracking - Measurement of the melt flow index - Carbon black and/or mineral filler content measurement in polyethylene by direct combustion - Measurement of carbon black content by thermogravimetric analysis (TGA) - Assessment of carbon black dispersion in polyethylene using a microscope |
EN 60811-1-2:1995/A2:2000 | INSULATING AND SHEATHING MATERIALS OF ELECTRIC CABLES - COMMON TEST METHODS - GENERAL APPLICATION - THERMAL AGEING METHODS |
IEC 60811-1-1:1993+AMD1:2001 CSV | Common test methods for insulating and sheathing materials of electric cables and optical cables - Part 1-1: Methods for general application - Measurement of thickness and overall dimensions - Tests for determining the mechanical properties |
EN 50290-2-30:2002 | Communication cables - Part 2-30: Common design rules and construction - Poly(tetrafluoroethylene-hexafluoropropylene) (FEP) insulation and sheathing |
EN 50395 : 2005 AMD 1 2011 | ELECTRICAL TEST METHODS FOR LOW VOLTAGE ENERGY CABLES |
EN 50290-2-25:2013 | COMMUNICATION CABLES - PART 2-25: COMMON DESIGN RULES AND CONSTRUCTION - POLYPROPYLENE INSULATION COMPOUNDS |
EN 60811-2-1 : 98 AMD 1 2001 | INSULATING AND SHEATHING MATERIALS OF ELECTRIC CABLES - COMMON TEST METHODS - PART 2-1: METHODS SPECIFIC TO ELASTOMERIC COMPOUNDS - OZONE RESISTANCE, HOT SET AND MINERAL OIL IMMERSION TESTS |
IEC 60811-1-3:1993+AMD1:2001 CSV | Common test methods for insulating and sheathing materials of electric and optical cables - Part 1-3: General application -Methods for determining the density - Water absorption tests - Shrinkage test |
EN 50290-2-22 : 2001 AMD 1 2007 | COMMUNICATION CABLES - PART 2-22: COMMON DESIGN RULES AND CONSTRUCTION - PVC SHEATHING COMPOUNDS |
IEC 60811-1-4:1985 | Common test methods for insulating and sheathing materials of electric cables - Part 1: Methods for general application - Section Four: Tests at low temperature |
IEC 60811-2-1:1998+AMD1:2001 CSV | Common test methods for insulating and sheathing materials of electric and optical cables - Part 2-1: Methods specific to elastomeric compounds - Ozone resistance, hot set and mineral oil immersion tests |
EN 50290-2-21:2001/A1:2007/AC:2016 | COMMUNICATION CABLES - PART 2-21: COMMON DESIGN RULES AND CONSTRUCTION - PVC INSULATING COMPOUNDS |
IEC 60811-3-2:1985 | Common test methods for insulating and sheathing materials of electric cables - Part 3: Methods specific to PVC compounds - Section Two: Loss of mass test - Thermal stability test |
EN 50267-2-2:1998 | Common test methods for cables under fire conditions - Tests on gases evolved during combustion of materials from cables - Part 2-2: Procedures - Determination of degree of acidity of gases for materials by measuring pH and conductivity |
EN 50290-2-24 : 2002 AMD 1 2008 | COMMUNICATION CABLES - PART 2-24: COMMON DESIGN RULES AND CONSTRUCTION - PE SHEATHING |
EN 50396 : 2005 AMD 1 2011 | NON ELECTRICAL TEST METHODS FOR LOW VOLTAGE ENERGY CABLES |
EN 60811-1-1:1995/A1:2001 | INSULATING AND SHEATHING MATERIALS OF ELECTRIC CABLES - COMMON TEST METHODS - GENERAL APPLICATION - MEASUREMENT OF THICKNESS AND OVERALL DIMENSIONS - TESTS FOR DETERMINING MECHANICAL PROPERTIES |
HD 604 S1:1994/A3:2005 | 0.6/1 KV POWER CABLES WITH SPECIAL FIRE PERFORMANCE FOR USE IN POWER STATIONS |
HD 621 S1:1996/A1:2001 | MV IMPREGNATED PAPER INSULATED DISTRIBUTION CABLES OF RATED VOLTAGES OF 3.8/6.6 KV TO 19/33 KV |
EN 60811-1-4:1995/A2:2001 | INSULATING AND SHEATHING MATERIALS OF ELECTRIC CABLES - COMMON TEST METHODS - PART 1-4: GENERAL APPLICATION - TESTS AT LOW TEMPERATURE |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.