I.S. EN 10346:2015
Current
The latest, up-to-date edition.
CONTINUOUSLY HOT-DIP COATED STEEL FLAT PRODUCTS FOR COLD FORMING - TECHNICAL DELIVERY CONDITIONS
Hardcopy , PDF
English
01-01-2015
For Harmonized Standards, check the EU site to confirm that the Standard is cited in the Official Journal.
Only cited Standards give presumption of conformance to New Approach Directives/Regulations.
Dates of withdrawal of national standards are available from NSAI.
European foreword
1 Scope
2 Normative References
3 Terms and definitions
4 Classification and designation
5 Information to be supplied by the purchaser
6 Manufacturing and processing
7 Requirements
8 Inspection
9 Marking
10 Packing
11 Storage and transportation
Annex A (normative) - Reference method for determination
of the zinc, zinc-iron, zinc-aluminium, zinc-magnesium
and aluminium-zinc coating mass
Annex B (normative) - Reference method for determination
of the aluminium-silicon coating mass
Annex C (normative) - Method for determination of the mass
of the Al-Fe-Si alloy layer
Annex D (informative) - Technical changes from the previous
edition
Bibliography
Describes requirements for continuously hot-dip coated products made of low carbon steels for cold forming, of steels for construction,and of steels with high proof strength for cold forming and coated with zinc (Z), zinc-iron alloy (ZF), zinc-aluminium alloy (ZA), aluminium-zinc alloy (AZ) or aluminium-silicon alloy (AS), and for continuously hot-dip coated products made of multiphase steels for cold forming coated with zinc (Z) zinc-iron alloy (ZF) or zinc-aluminium alloy (ZA) with thicknesses of 0,20<= t < 3,0 mm.
DevelopmentNote |
Supersedes I.S. EN 10292, I.S. EN 10326, I.S. EN 10327 & I.S. EN 10336. (05/2009)
|
DocumentType |
Standard
|
Pages |
44
|
PublisherName |
National Standards Authority of Ireland
|
Status |
Current
|
Supersedes |
Standards | Relationship |
EN 10346:2015 | Identical |
S.R. 70:2015 | TIMBER IN CONSTRUCTION - EUROCODE 5 - TRUSSED RAFTERS |
ISO 10275:2007 | Metallic materials Sheet and strip Determination of tensile strain hardening exponent |
EN 10079:2007 | Definition of steel products |
EN 10027-2:2015 | Designation systems for steels - Part 2: Numerical system |
EN 10152:2017 | Electrolytically zinc coated cold rolled steel flat products for cold forming - Technical delivery conditions |
EN ISO 6892-1:2016 | Metallic materials - Tensile testing - Part 1: Method of test at room temperature (ISO 6892-1:2016) |
ISO 14713-1:2017 | Zinc coatings — Guidelines and recommendations for the protection against corrosion of iron and steel in structures — Part 1: General principles of design and corrosion resistance |
ISO 6892-1:2016 | Metallic materials Tensile testing Part 1: Method of test at room temperature |
EN 10149-2:2013 | Hot rolled flat products made of high yield strength steels for cold forming - Part 2: Technical delivery conditions for thermomechanically rolled steels |
EN 10169:2010+A1:2012 | Continuously organic coated (coil coated) steel flat products - Technical delivery conditions |
EN 10143:2006 | Continuously hot-dip coated steel sheet and strip - Tolerances on dimensions and shape |
EN 10021:2006 | General technical delivery conditions for steel products |
EN ISO 14713-1:2017 | Zinc coatings - Guidelines and recommendations for the protection against corrosion of iron and steel in structures - Part 1: General principles of design and corrosion resistance (ISO 14713-1:2017) |
EN 10204:2004 | Metallic products - Types of inspection documents |
EN 10049:2013 | Measurement of roughness average Ra and peak count RPc on metallic flat products |
EN 10027-1:2016 | Designation systems for steels - Part 1: Steel names |
ISO 10113:2006 | Metallic materials Sheet and strip Determination of plastic strain ratio |
EN 10020:2000 | Definition and classification of grades of steel |
EN 606:2004 | Bar coding - Transport and handling labels for steel products |
ISO 14713-2:2009 | Zinc coatings Guidelines and recommendations for the protection against corrosion of iron and steel in structures Part 2: Hot dip galvanizing |
EN 10325:2006 | Steel - Determination of yield strength increase by the effect of heat treatment [Bake-Hardening-Index] |
EN ISO 14713-2:2009 | Zinc coatings - Guidelines and recommendations for the protection against corrosion of iron and steel in structures - Part 2: Hot dip galvanizing (ISO 14713-2:2009) |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.